Welcome to the world’s most advanced solar backsheet product directory. Panel manufacturers can use our advanced technical filters to find the exact solar backsheet that matches their needs. We have collated backsheet data from manufacturers from all around the world into a common template, allowing you to compare and review backsheets easily.
Layers: | PET / PET / Primer | Tensile Strength: | -- |
Total Thickness: | 295±14.75 µm | Thermal Shrinkage: ≤ | 1.2 % |
Region: | Italy |
Layers: | -- | Tensile Strength: | 100 MPa |
Total Thickness: | 295 µm | Thermal Shrinkage: ≤ | 1 % |
Region: | China |
Layers: | PET / PET / Primer | Tensile Strength: | -- |
Total Thickness: | 295±14.75 µm | Thermal Shrinkage: ≤ | 1.2 % |
Region: | Italy |
Layers: | PVF / PET / Primer | Tensile Strength: | 100 MPa |
Total Thickness: | 320 µm | Thermal Shrinkage: ≤ | 1.5 % |
Region: | India |
Layers: | PVDF / PET / FFC | Tensile Strength: | 167 MPa |
Total Thickness: | 300±15 µm | Thermal Shrinkage: ≤ | 0.41 % |
Region: | China |
Layers: | THV / PET / EVA | Tensile Strength: | 38 MPa |
Total Thickness: | 360 µm | Thermal Shrinkage: ≤ | 1.2 % |
Region: | United States |
Layers: | FFC / PET / FFC | Tensile Strength: | 168 MPa |
Total Thickness: | 300±15 µm | Thermal Shrinkage: ≤ | 0.45 % |
Region: | China |
Layers: | Coating / PET / Coating | Tensile Strength: | 190 MPa |
Total Thickness: | 170 µm | Thermal Shrinkage: ≤ | 1.5 % |
Region: | Germany |
Layers: | PET / PET / EVA | Tensile Strength: | 120 MPa |
Total Thickness: | 300±10 µm | Thermal Shrinkage: ≤ | 1 % |
Region: | China |
Layers: | PVDF / PET / PVDF | Tensile Strength: | 172 MPa |
Total Thickness: | 316±15.8 µm | Thermal Shrinkage: ≤ | 0.53 % |