Welcome to the world’s most advanced solar backsheet product directory. Panel manufacturers can use our advanced technical filters to find the exact solar backsheet that matches their needs. We have collated backsheet data from manufacturers from all around the world into a common template, allowing you to compare and review backsheets easily.
Layers: | PET / PET / Primer | Tensile Strength: | 90 MPa |
Total Thickness: | 300±5 µm | Thermal Shrinkage: ≤ | 1.5 % |
Region: | India |
Layers: | Tedlar(PVF) / PET / EVA | Tensile Strength: | 77 MPa |
Total Thickness: | 323±32.3 µm | Thermal Shrinkage: ≤ | 1.5 % |
Region: | United States |
Layers: | Coating / PET / Coating | Tensile Strength: | 183 MPa |
Total Thickness: | -- | Thermal Shrinkage: ≤ | -- |
Region: | Korea |
Layers: | FEVE / PET / PTFE | Tensile Strength: | 160 MPa |
Total Thickness: | 300±50 µm | Thermal Shrinkage: ≤ | 2 % |
Region: | China |
Layers: | PET / PET / Primer | Tensile Strength: | 90 MPa |
Total Thickness: | 295 µm | Thermal Shrinkage: ≤ | 1.5 % |
Region: | India |
Layers: | PET / PET / Primer | Tensile Strength: | 100 MPa |
Total Thickness: | 320 µm | Thermal Shrinkage: ≤ | 1.5 % |
Region: | India |
Layers: | PVF / PET / PE | Tensile Strength: | 100 MPa |
Total Thickness: | 355 µm | Thermal Shrinkage: ≤ | 1 % |
Region: | China |
Layers: | Polyester / Polyester | Tensile Strength: | 140 MPa |
Total Thickness: | 370 µm | Thermal Shrinkage: ≤ | 0.8 % |
Region: | Germany |
Layers: | Coating / PET / Coating | Tensile Strength: | -- |
Total Thickness: | 270 µm | Thermal Shrinkage: ≤ | 0.3 % |
Region: | China |
Layers: | Coating / PET / Coating | Tensile Strength: | -- |
Total Thickness: | 145 µm | Thermal Shrinkage: ≤ | 0.3 % |
Region: | China |