Solar Backsheet Directory

Welcome to the world’s most advanced solar backsheet product directory. Panel manufacturers can use our advanced technical filters to find the exact solar backsheet that match their needs. We have collated backsheet data from manufacturers from all around the world into a common template, allowing you to compare and review backsheets easily. Finally, please also note that on the left side of the page you can select the backsheet layer materials you are looking for.

Browse by

Region

Outer(Air)Layer

Mid Layer

Inner(Cell)Layer

Tensile Strength(Width/TD) ≥

Mpa

Interlayer Peel Strength ≥

N/cm

Thermal Shrinkage(Width/TD) ≤

%

Elongation(Length/MD) ≥

%

Elongation(Width/TD) ≥

%

Partial Discharge Voltage ≥

VDC

Breakdown Voltage ≥

kV

MVTR ≤

g/m2 per day

Width ≥

mm

Weight ≤

g/m2

Solar Backsheet Directory
(119 Individual Backsheet Models)

Backsheet Filters
µm µm
MPa MPa
%
N/cm N/cm
  • Protekt® HD
    Layers: Coating / Polyester / EVA Tensile Strength: 112 MPa
    Total Thickness: 249±25 µm Thermal Shrinkage ≤: --
    Region: United States United States    
  • KFB-30
    Series: KFB-30
    Jolywood (Suzhou) Sunwatt
    Layers: PVDF / PET / FFC Tensile Strength: 167 MPa
    Total Thickness: 300±15 µm Thermal Shrinkage ≤: 0.41 %
    Region: China China    
  • Scotchshield Film 15T
    Layers: THV / PET / EVA Tensile Strength: 38 MPa
    Total Thickness: 360 µm Thermal Shrinkage ≤: 1.2 %
    Region: United States United States    
  • Scotchshield Film 15T Black
    Layers: THV / PET / EVA Tensile Strength: 45 MPa
    Total Thickness: 360 µm Thermal Shrinkage ≤: 1.2 %
    Region: United States United States    
  • FLEXcon multiGUARD TPT 12
    Layers: Tedlar(PVF) / PET / Tedlar(PVF) Tensile Strength: 149 MPa
    Total Thickness: 323±32.3 µm Thermal Shrinkage ≤: 1.5 %
    Region: United States United States    
  • Reflekt® Lean 300
    Layers: Coating / PET / Polyolefin Tensile Strength: 83 MPa
    Total Thickness: 345 µm Thermal Shrinkage ≤: --
    Region: United States United States    
  • PVDF for backsheet
    Series: PVDF for backsheet
    HIUV New Materials
    Layers: PVDF / PET / PVDF Tensile Strength: --
    Total Thickness: 25 µm Thermal Shrinkage ≤: 2 %
    Region: China China    
  • dyMat APYE
    Layers: PET / AL / PET / Primer Tensile Strength: --
    Total Thickness: 370±18.5 µm Thermal Shrinkage ≤: 1 %
    Region: Italy Italy    
  • TFB-40
    Series: TFB-40
    Jolywood (Suzhou) Sunwatt
    Layers: PVF / PET / FFC Tensile Strength: 183 MPa
    Total Thickness: 395±19.75 µm Thermal Shrinkage ≤: 0.54 %
    Region: China China    
  • neoX CPC 150
    Layers: Coating / PET / Coating Tensile Strength: 190 MPa
    Total Thickness: 170 µm Thermal Shrinkage ≤: 1.5 %
    Region: Germany Germany